Premixed plaster used for light weight concrete block work. Available both indoor and outdoor. Also can be used for wall plastering work. Mon brick or concrete blocks as well.
Compound material between TPI Portland cement Crushed stone through the drying process and size up to 2 times and high quality chemicals from abroad. It has special properties for waterproofing. And cracking sesame Wall not slip And do not shrink after plastering. Suitable for a variety of applications. Just mix the water to the right proportion, it can be used immediately.
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 10/ 2.88/ 17
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 15/ 2.16/ 23
Ready-mixed plaster for general plastering Suitable for use with brick wall brick mon Or concrete block Available both indoor and outdoor. Certified according to TIS 1776-2566 (General Putty)
Compound material between TPI Portland cement Crushed stone through the drying process and size up to 2 times and high quality chemicals from abroad. It has special properties for waterproofing. And cracking sesame Wall not slip And do not shrink after plastering. Suitable for a variety of applications. Just mix the water to the right proportion, it can be used immediately.
- Clean and pour the water to the wall to be plastered to moderate.
- Mix TPI (M200) concrete with 3.5: 1 volume of clean water.
- Mix well.
- Apply to the general putty. It can also be used in conjunction with a Mortar Machine.
- Mixing 1 bag of water 11 liters
- Weight 50 k.g.
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 10/2.88/ 17
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 15/ 2.16/ 23
Finished fine morter used for plastering, such as concrete walls, both inside and outside the building, is certified according to Thai Industrial Standard Institute 1776-2566 (Putty Cement).
Compound material between TPI Portland cement Crushed stone through the drying process and size up to 2 times and high quality chemicals from abroad. Special properties in water. Extra high adhesion strength. The plaster texture is easy to slip plaster, reduce the problem of cracking. And cracking sesame Wall not slip And do not shrink after plastering. Suitable for a variety of applications. Just mix the water to the right proportion, it can be used immediately.
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 5/ 5.75/ 8.7
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 10/ 2.89/ 17.3
Finished plaster used for wall decoration that requires exquisite workmanship, the work will be smooth and fine. Suitable for mon brick wall. Or concrete block Both indoor and outdoor use. TIS 1776-2566 (Plate)
Compound material between TPI Portland cement Crushed stone through the drying process and size up to 2 times and high quality chemicals from abroad. It has special properties for waterproofing. And cracking sesame Wall not slip And do not shrink after plastering. Suitable for a variety of applications. Just mix the water to the right proportion, it can be used immediately.
Thickness (m.m.)/ Mortar 1 plastered canvas (sq.m.)/ Usage per square meter (k.g.) 10/ 2.88/ 17
Thickness (m.m.) Mortar 1 plastered canvas (sq.m.) Usage per square meter (k.g.) 15/ 2.16/ 23
TPI M319 is an instant masonry mortar which is formulated for Lightweight block mansory work. It is providing high adhesion strength, excellent workability and easy to use. The finished walls are high durability strength.
|
How to prepare |
|
Precast concrete especially developed for lightweight concrete blocks. High adhesion to slippery, easy to work quickly. Make the walls beautiful and strong.
Material used/ Thickness (mm)/ 1 bag of cement mortar area (cm)/ Usage per square meter (kg)
Lightweight block mortar/ Only 3-5 floors/ 7.5x20x60/ 30
A ready – dry mixed mortar suitable for masonry work both indoor and outdoor application such as bricklaying of brick or concrete block (but not including lightweight block) It is providing a high adhesive strength, good workability. It conforms to TIS 598 – 2566 Thai industrial standard for (Masonry ready dry mixed mortar (type50))
Ready-to-use mortar Used for internal wall and wall work. Externally above ground level buildings such as mon brick walls or concrete blocks. (But not including aerobics blocks) that enhance adhesion. Make the wall more convenient. Both are still in compliance with TIS 598-2566, dry mortar (type 50)
Material used/ 1 bag of cement mortar area (sq.m) /Usage per square meter (kg)
Brick Masonry (6x14x3 cm.)/ 1.15/ 43.48
Brick Holes (6.5x16x4 cm.)/ 1.25/ 40.00
Concrete Block (39x19x7 cm.)/ 2.00/ 25.00
Polene Solar® ผลิตจากเม็ดพลาสติก Polene® EVA และส่วนผสมของสารเติมแต่งพิเศษ ที่ช่วยให้เกิดโครงสร้างแบบร่างแหซึ่งมีความแข็งแรงสูง (Cross-Linking) เหมาะสำหรับการผลิตแผงพลังงานแสงอาทิตย์ทั้งชนิด Crystalline และ Amorphous Thin Film
ผลิตภัณฑ์ Polene Solar® พัฒนาขึ้นด้วยเทคโนโลยีขั้นสูง โดยความร่วมมือระหว่างผู้ผลิตแผงพลังงานแสงอาทิตย์ชั้นนำในประเทศไทย และทีมวิจัยพัฒนาที่มีความรู้และประสบการณ์ด้านพอลิเมอร์มานานกว่า 10 ปี
This is designed to render high early compressive strength. It is manufactured in accordance with the Thai Industrial Standards Institute's specification for portland cement TIS 15 - 2547 Type 3 and the American ASTM C-150 Type III.
Property : Suitable for the use in concrete work which requires support strength and quick setting as well as for the manufacturing of all prestressed concrete products, e.g. concrete piles, floor slabs, beams, and pylons.
|
According to the American Standard Specification for |
Guarantee Specification |
||
|
ASTM C 114 |
|
|
| Silicon dioxide |
(SiO2) |
% |
- |
|
Aluminium oxide |
(AI2O3) |
% |
- |
|
Ferric oxide |
(Fe2O3) |
% |
- |
|
Calcium oxide |
(CaO) |
% |
- |
|
Magnesium oxide |
(MgO) |
% |
max 6.0 |
|
Sulfur trioxide |
(SO3) |
% |
max 3.5 |
|
Loss of ignition |
(LOI) |
% |
max 3.0 |
|
Insoluble residue |
(IR) |
% |
max 0.75 |
|
Tricalcium silicate |
(C3S) |
% |
- |
|
Tricalcium aluminate |
(C3A) |
% |
max 15 |
| Total Alkalies (Na2O + 0.658 K2O) |
max 0.6 |
||
|
|
||
|
Fineness ; Specific surface Air permeability test |
ASTM C 204 |
m2/kg |
- |
|
Soundness : Autoclave expansion |
ASTM C 151 |
% |
max 0.8 |
|
Time of setting ; Vicat test; |
ASTM C 191 |
||
|
initial set |
mins |
min 45 |
|
|
final set |
mins |
max 375 |
|
|
Air content of mortar volume |
ASTM C 185 |
% |
max 12 |
|
*False set |
ASTM C 451 |
% |
min 50 |
|
Compressive Strength ; Mortar cubes; |
ASTM C 109 |
psi (MPa)[ksc] |
|
|
1 day |
min 1740 (12.0)[122] |
||
|
3 days |
min 3480 (24.0)[245] |
||
|
7 days |
- |
||
|
28 days |
- |
||
Remark : * Means Optional Requirements